{"number":"US12702901B2","kindCode":"B2","documentType":"grant","title":{"original":"Method for single-step heat treatment of titanium alloys, golf club striking faces, and golf club heads","english":"Method for single-step heat treatment of titanium alloys, golf club striking faces, and golf club heads"},"abstract":{"original":"A method for manufacturing a golf club head includes forming a pre-forged striking face insert from an α-β titanium alloy having a Molybdenum equivalency of about 6 to 12 or an Al equivalency of about 2 to 7, and forging the pre-forged striking face insert into a forged striking face insert having a specified geometry or curvature.…","english":"A method for manufacturing a golf club head includes forming a pre-forged striking face insert from an α-β titanium alloy having a Molybdenum equivalency of about 6 to 12 or an Al equivalency of about 2 to 7, and forging the pre-forged striking face insert into a forged striking face insert having a specified geometry or curvature.…"},"applicants":["Acushnet Company"],"inventors":["Uday V. Deshmukh","Jorgen Meister"],"filingDate":"2023-12-21","publicationDate":"2026-08-11","grantDate":"2026-08-11","verifiedWithOffice":true,"pdfUrl":"https://downloadpatent.com/pdf/US12702901B2.pdf","pages":{"en":"https://downloadpatent.com/patent/US12702901B2","zh-Hant":"https://downloadpatent.com/zh-Hant/patent/US12702901B2","ja":"https://downloadpatent.com/ja/patent/US12702901B2"}}